Corrosion of reinforcement causes cracking and spalling of concrete cover mainly because:
सही उत्तर: घ) The rust formed occupies a much larger volume than the original steel
Iron oxides occupy several times the volume of the steel consumed, so the expansion bursts the surrounding concrete.
💬 टिप्पणी / गल्ती रिपोर्ट (०)
-
Hardening of steel is done by heating it above the critical temperature and then:
सही उत्तर: ग) Cooling it rapidly by quenching in water or oil
Rapid quenching forms hard martensite; slow furnace cooling is annealing and air cooling is normalising.
💬 टिप्पणी / गल्ती रिपोर्ट (०)
-
A TMT reinforcing bar, as a result of quenching followed by self-tempering, has:
सही उत्तर: ख) A hard tempered martensite outer rim and a soft, ductile ferrite-pearlite core
Quenching hardens the surface into martensite, which is tempered by heat from the core, leaving a tough ferrite-pearlite core.
💬 टिप्पणी / गल्ती रिपोर्ट (०)
-
CRS bars used as reinforcement in aggressive environments are:
सही उत्तर: क) Corrosion resistant steel bars
CRS bars contain small amounts of alloying elements such as copper, chromium or phosphorus to improve resistance to corrosion.
💬 टिप्पणी / गल्ती रिपोर्ट (०)
-
The suffix 'D' in reinforcement grades such as Fe 500D indicates bars with:
सही उत्तर: घ) Higher ductility, with greater elongation and stricter limits on sulphur and phosphorus
D-grade bars have enhanced ductility requirements, which is useful in earthquake-resistant construction.
💬 टिप्पणी / गल्ती रिपोर्ट (०)
-
As per IS 1786, the minimum ultimate tensile strength of Fe 415 reinforcing bars is:
सही उत्तर: ग) 485 N/mm²
Fe 415 must have a tensile strength of at least 485 N/mm² (and at least 10% above its actual proof stress).
💬 टिप्पणी / गल्ती रिपोर्ट (०)
-
The steel-making furnace that uses mainly steel scrap as its charge, melted by electricity, is the:
सही उत्तर: ख) Electric arc furnace
An electric arc furnace melts scrap (and sponge iron) using an electric arc between graphite electrodes.
💬 टिप्पणी / गल्ती रिपोर्ट (०)
-
Timber is weakest when loaded in:
सही उत्तर: क) Tension perpendicular to the grain
The fibres are held together only weakly across the grain, so tension perpendicular to the grain is its weakest direction.
💬 टिप्पणी / गल्ती रिपोर्ट (०)
-
Glulam (glued laminated timber) consists of:
सही उत्तर: घ) Several layers of dimension lumber glued together with grains parallel to form large structural members
In glulam, laminations are glued with grains parallel, allowing long, strong and curved beams to be made.
💬 टिप्पणी / गल्ती रिपोर्ट (०)
-
Charring the lower ends of wooden posts before embedding them in the ground is done to:
सही उत्तर: ग) Protect them from decay and insects by forming a carbonised layer
The charred layer is not attacked readily by fungi and insects, giving a simple form of preservation.
💬 टिप्पणी / गल्ती रिपोर्ट (०)
यी अभ्यास प्रश्न हुन्, आधिकारिक प्रश्न होइनन्। पाठ्यक्रम, विज्ञापन र नतिजाका लागि सम्बन्धित निकायको आधिकारिक वेबसाइट हेर्नुहोस्। उत्तरमा गल्ती भेटे प्रश्नमुनिको "टिप्पणी / गल्ती रिपोर्ट" मा लेख्नुहोस्।
नमस्ते! पाठ्यक्रम, सामान्य ज्ञान, भाषा परीक्षा वा कुनै प्रश्नको उत्तर बुझ्न सोध्नुहोस्।
AI ले गल्ती गर्न सक्छ। महत्वपूर्ण कुरा आधिकारिक स्रोतमा जाँच्नुहोस्।