Tempering of steel, done after hardening, consists of:
सही उत्तर: ग) Reheating to a moderate temperature and cooling, to reduce brittleness
Hardened steel is very brittle; tempering at a lower temperature relieves stresses and restores some toughness.
💬 टिप्पणी / गल्ती रिपोर्ट (०)
-
In the designation ISMB 300 for a rolled steel section, 'ISMB' stands for:
सही उत्तर: क) Indian Standard Medium weight Beam
ISMB is an I-section medium weight beam; the number gives its depth in millimetres.
💬 टिप्पणी / गल्ती रिपोर्ट (०)
-
As per IS 1786, the minimum percentage elongation required for Fe 415 bars is:
सही उत्तर: ख) 14.5%
IS 1786 specifies minimum elongation of 14.5% for Fe 415 and 12% for Fe 500.
💬 टिप्पणी / गल्ती रिपोर्ट (०)
-
Ribbed (deformed) reinforcement bars are preferred over plain round bars mainly because they give:
सही उत्तर: ख) Better bond with concrete
The ribs mechanically interlock with concrete, greatly increasing bond strength and reducing the anchorage length needed.
💬 टिप्पणी / गल्ती रिपोर्ट (०)
-
High carbon steel is most suitable for:
सही उत्तर: घ) Cutting tools, springs and drills
High carbon steel (about 0.6–1.5% C) can be hardened to a high degree, which suits tools and springs.
💬 टिप्पणी / गल्ती रिपोर्ट (०)
-
As the carbon content of plain steel increases, its:
सही उत्तर: क) Hardness and strength increase but ductility decreases
More carbon makes steel harder and stronger but less ductile and less weldable.
💬 टिप्पणी / गल्ती रिपोर्ट (०)
-
The LD (basic oxygen) process of steel making involves:
सही उत्तर: ख) Blowing pure oxygen onto molten pig iron in a converter
In the Linz-Donawitz process, high-purity oxygen is blown onto the molten charge, burning out carbon and impurities quickly.
💬 टिप्पणी / गल्ती रिपोर्ट (०)
-
The product obtained from a blast furnace by smelting iron ore with coke and limestone is:
सही उत्तर: घ) Pig iron
The blast furnace produces pig iron (with about 3–4% carbon), which is then refined into cast iron, wrought iron or steel.
💬 टिप्पणी / गल्ती रिपोर्ट (०)
-
The moisture content of timber at site is quickly measured using a:
सही उत्तर: ख) Moisture meter based on electrical resistance
Electrical moisture meters estimate moisture content from the resistance between two pins driven into the wood.
💬 टिप्पणी / गल्ती रिपोर्ट (०)
-
Sissoo, a dense and durable timber widely used for furniture in the Terai of Nepal, has the botanical name:
सही उत्तर: घ) Dalbergia sissoo
Sissoo is Dalbergia sissoo; Shorea robusta is sal, Tectona grandis is teak and Pinus roxburghii is chir pine.
💬 टिप्पणी / गल्ती रिपोर्ट (०)
यी अभ्यास प्रश्न हुन्, आधिकारिक प्रश्न होइनन्। पाठ्यक्रम, विज्ञापन र नतिजाका लागि सम्बन्धित निकायको आधिकारिक वेबसाइट हेर्नुहोस्। उत्तरमा गल्ती भेटे प्रश्नमुनिको "टिप्पणी / गल्ती रिपोर्ट" मा लेख्नुहोस्।
नमस्ते! पाठ्यक्रम, सामान्य ज्ञान, भाषा परीक्षा वा कुनै प्रश्नको उत्तर बुझ्न सोध्नुहोस्।
AI ले गल्ती गर्न सक्छ। महत्वपूर्ण कुरा आधिकारिक स्रोतमा जाँच्नुहोस्।